6x6mm square ingot mold

I have been on the hunt for an ingot mold that will produce 6 x 6 mm square ingots about 8-12 inches in length. I just purchased an electric rolling mill and the widest it will open is 6 mm. Im kinda tired of making short pieces of Sterling wire and would hope to be able to make longer pieces so I can create my Cuban link bracelets and necklaces. 2023-08-01T05:00:00Z

Hans Meevis has instructions on how to make an ingot mold, or you can buy one from him. See:

and:

Instructions to make one: