I have a CMF 1200 for sale, I don’t do manufacturing any longer.
Most jewelers I know here can’t use this. It is a Raytech CMF 1200
Centrifugal Magnetic Finisher. Good condition. Asking 1200.00 +
shipping. If you have specific questions just google for specs, etc.
Would be great to move this on to someone who can use it.