HI all I picked up a ring today with the marking 141 in a rectangular
box… Anyone familiar with this marking or hallmark? Thanks Paul
DeFruscio

Most likely it is a 14k stamp that didn’t quite stamp out properly.

Daniel R. Spirer, G.G.
Spirer Somes Jewelers
1794 Massachusetts Ave.
Cambridge, MA 02140
617-491-6000
www.spirersomes.com