I used to clean my piano keys with a solution of vinegar & warm
water - this would also, marginally, whiten the yellow.
Jan MacLellan
Burnaby, Canada
I used to clean my piano keys with a solution of vinegar & warm
water - this would also, marginally, whiten the yellow.
Jan MacLellan
Burnaby, Canada
This is an official retraction folks…my brain told my
fingers to type the wrong thing. In my last post I said that
Ivory is 70% Calcium Carbonate. It ain’t so. Ivory is 70%
Calcium Phosphate. Please forgive my mistake (and be glad that I
don’t write the tech manuals for your local Breeder Reactor.)

-Pete-
Buffalo, NY, (Northeast USA, near the Great Lakes)