you say not to get the yellow ochre in the pickel pot but what about the
white out? will it cause a problem! i like this solution but the extra
step of cleaning the y o first takes time.

thanks,
david horn


#2

At 08:54 AM 11/2/96 -0500, you wrote:

you say not to get the yellow ochre in the pickel pot but what about the
white out? will it cause a problem! i like this solution but the extra
step of cleaning the y o first takes time.

thanks,
david horn

I/ve not had any problems with the white out contaminating my pickle pot; no
iron oxides to cause any problems and the amount you use is so small it
doesn’t even cause clouding of the pickle.

Susan

C Gems
Original Designs and Period Jewelry
cgems@pipeline.com