Hi Don,
Alas, I haven’t been able to actually start the piece because I’ve been backed up on commissions, followed by an out of town business trip. Hope to get rolling at the end of the month. I looked through my photos and don’t have anything on the inside of the piece. What I remember is a small piece of wire soldered in place just beneath the inner edge as the beginning of the wrap. Each wrap then covered this little piece until the end where again a small amount of wire was tucked and soldered in place. I have plenty of extra wire and silver sheet to do a small test piece before taking on the bigger cuff. Will share my progress with the group as soon as I get started.
Thanks so much for following up with me!
Sally