Hello all - I went to a seminar last spring and discovered “wizard
wax” as it was used for the Roland Mills and ProtoWizard hardware.
Have any of your used this wizard wax to actually hand carve models ?
It seems to be very hard and flaky, much harder than Ferris green
carving wax. The color of this wax is orange, which would make it
hard
for eyes of my age and years of close up work harder to see details.

Just curious about flex, memory and ability to do build-up work.

Margie
www.deepdetail.com

I have used the wizard wax on my 3D mill and it does give great
detail but it is brittle also. You need to be careful when handling
it. I still prefer the purple wax myself even on my mill.