Hi Kathy , This is really a form of depletion gilding . As I
understand the process , the pickle is leaching the surface copper
from the sterling and leaving pure silver . I,ve done this to hide
firescale ! The silver is still the same , its just a very thin layer
on top . Best wishes , Philip Wells in cold , sunny Nelson