There are two choices from stuller one being the new X1 white gold,
as well the bright white from stuller which has a 13 percent nickel
content. it also needs no plating.

Andy " The Tool Guy" Kroungold
Tool Sales / Technical
Stuller Inc
Phone 800-877-7777 ext. 94194
Fax 337-262-7791

Andy is correct. Stuller’s new Rhodium-Free White Gold is here, and
available in 10K, 14K, 18K, and even 19K White casting grain.

James Gilbert
Stuller Metals

Andy is correct. Stuller's new Rhodium-Free White Gold is here, and
available in 10K, 14K, 18K, and even 19K White casting grain.

Is this only a cast product or is it available as wrought material?

Jim Binnion

James Binnion Metal Arts
Phone (360) 756-6550
Toll Free (877) 408 7287
Fax (360) 756-2160


@James_Binnion
Member of the Better Business Bureau

    Is this only a cast product or is it available as wrought
material? 

Jim: Stuller’s new X1 white gold is currently offered in casting
grain only (10K, 14K, 18K, and 19K). However, we will announce a mill
product offering that includes sheet, wire, sizing stock, and solders
by this summer. Interestingly, this product performs exceptionally
well in sheet production and wire drawing applications. Stuller has
run production and fabrication tests on the mill products with
excellent results. Grain structure control elements provide good
mechanical characteristics as well as improved grain structure and
surface finish.

Give me a call at extension 6113 if you would like more info, or
would like to place an order for mill products now. I am familiar
with your work, and would enjoy discussing with you…Thanks!

James Gilbert
Stuller Metals
800-877-7777