White gold melting point

 If I can melt white gold at that temperature, is it possible to
add yellow gold alloy to the white to produce a colour in between
the two? 

Hi Karl, You can definitely mix white gold with yellow, but you get
an ugly color, no matter what the proportions.

Tom Arnold