anyone tried the warrior jewelry package for polishing lap. It uses
the ninja disc by 3M… Just curious.

Frank Goss

anyone tried the warrior jewelry package for polishing lap. It uses
the ninja disc by 3M. 

Yes and I was not very happy with it. The Ninja sanding disks are
not very flat so you only use abrasive from spots on the disc and the
die cut sanding discs are rather pricey. Ill be happy to sell my
system to anyone who wants to take it off my hands. I ma a tool
junkie and virtually never get rid of a tool this tells you what I
think of it.