Greetings Microbiologist: You have convinced me that verdigris is
nasty stuff. Is it safe for the wearer to put a green patina on
bronze, brass or shibuichi? Is it safe if the patina is covered with
lacquer or varnish? I’ve seen beautiful green and blue patinas on
jewelry, but are the jewelers promoting a dangerous product?
Sally Parker