I had a similar problem with a pair of earring I made, the one hole
looked out of place. I decided to drill more holes and use the them
to design different constellations. Each hole was a star in the
constellation. Sometimes I gypsy set stones with that design when I
use thicker sheet metal and it looks really cool. Hope that might
help.