Using milgrain tools?

Thank you. that was very clear and easy to understand. How do you
bright cut? Jo H. said she bright cuts the edge of her bezels before
she pushes them all the way down, but Im not sure what bright
cutting is?

Leslie

but Im not sure what bright cutting is? 

Bright cutting is cutting with graver that has been polished to
mirror finish. Such graver leaves highly polished surface with no
farther polishing required.

Leonid Surpin