Back to Ganoksin | FAQ | Contact

[Tutorial] Adding color to Titanium with a Torch


#1

Hi!

I just finished a Tutorial called, Adding color to Titanium with a
Torch:

http://hollygage.com/pages/adding_color_to_titanium_with_a_torch.html

This technique is great for adding color to natural or rather
uncolored Titanium to give it brilliant color, alter the color on a
piece of existing Titanium, or change Titanium Seconds

http://www.hollygage.com/pages/purchase_seconds_titanium.html

Let me know if you find this helpful.
Holly


#2
http://hollygage.com/pages/adding_color_to_titanium_with_a_torch.html
http://www.hollygage.com/pages/purchase_seconds_titanium.html 

Hi Holly, Thank you ive never worked with Titanium and just starting
to learn how to change colours ect. :slight_smile:

Anthony Galea Designer Jeweller