Torch enamelling may be fine for small non perfect items, but ti
achieve high quality enamelling a kiln is a must. None of my
professional enameller friends here in the UK do torch fired
enamels. How could you achieve this quality of enamelling with a
torch?
Peace and good health to all metalsmiths James Miller FIPG