A short slideshow depicting the development of a torch-fired enamel piece. - See this video on Photobucket.

I learned how to enamel with a torch at a workshop given by Chris
Hierholzer to the FSGNE (Florida Society of Goldsmiths, NE Chapter),
last month. Being happily ignorant of the pitfalls, I made a
cloissone piece with flattened copper wires on a domed copper disk.

The slideshow has been posted to photobucket. If the above link
doesn’t work, go to my account, dragonwerx, to see the stages of
cloissone development.