Howdy,

Anyone utilized the TI research casting machine. Looks like a white
metal casting machine. Web site is ti-research.de

Howdy,

Anyone utilized the TI research casting machine. Looks like a white
metal casting machine. Web site is ti-research.de

Dear Steve,

All I can say after looking at Ti-research’s website is WOW!! Thank
you for bringing it to our attention.

Ed Katz, G.G., Jewels and Tools,
15434 Rio Plaza, Houston TX 77083

I haven’t used one but I did contact them because it looks like a
good unit. It is quite expensive I belive it was about $4000. If it
were less expensive I would be interested in trying it There are
some advantages to this type of centrifugal casting setup but I am
not sure they are worth the cost.

Jim Binnion