Back to Ganoksin | FAQ | Contact

There are rubber warts inside the mold

Jim, you don’t need any special metal to make a good rubber mold. I
have seen warts in Castaldo Gold Label a few times over the years. It
happens once in a while in Castaldo. Just use Flex Grade rubber from
Zero-D. You will not have the warts anymore. Call them at
1-800-382-3271

Craig