Back to Ganoksin | FAQ | Contact

The fodiator bow unabridged and naked


#1

I just finished my latest project which I call The Fodiator bow.

It’s a fantasy piece that has a miniature hidden cross bow in the
wings.

Three hundred and seven pieces and three months work and set with
amethysts, peridots,citrines, garnets and aquamarines.

Made out of silver, brass, copper and steel.

Check out my Orchid Blog at
http://www.ganoksin.com/gnkurl/ep80je

meevis.com


#2

Fantastic!


#3

Hans, I am once again blown away by your fertile imagination.

Dennis Fisher


#4

Some C. E.O. is going to have a nice toy. Wow well done, sir.

Teri


#5

You have done it again, Hans. An amazing construction of an
imaginary creature with a hidden “talent”, and wonderful to look at
as well! I thought your Dragon was. well… as rare as hen’s teeth.
Now it has a companion.

Thanks for sharing, and do you ever sleepe?

Judy in Kansas, where chickens are pretty common, but hen’s teeth?
Not so much.


#6

Hans you are an incredible craftsman with an incredible imagination
and talent. And great sense of humor. Thank you for sharing on
Orchid. Amanda


#7

Holy flyin’ carp, Hans! You never cease to amaze. If you ever bring
the fodiator to the states, you’ll find a very target rich
environment. Bring lots of bolts, please!

Thanks for sharing!

Dave Phelps


#8

Hans, this is so cool and my statement seems very understated. way
to go!

Kay Cummins


#9

I think it’s wonderful that you’re able to make such fun works of
art.


#10

Seriously wicked! I love your use of copper and brass, awesome
materials with such a rich history. Oh, and the spikes, I love the
spikes!

Kaleb


#11

(making Wayne & Garth obeisance)
We are not worthy! We are not worthy!

Elliot Nesterman


#12

Would someone let me know how to find this “fodiator” thing? What
day was it posted? I looked and can’t find it. Sounds like it was
quite a hit! Thanks! Marianne


#13
Would someone let me know how to find this "fodiator" thing? What
day was it posted? I looked and can't find it. Sounds like it was
quite a hit! 

Here’s his original post:

I just finished my latest project which I call The Fodiator bow.

It’s a fantasy piece that has a miniature hidden cross bow in the
wings.

Three hundred and seven pieces and three months work and set with
amethysts, peridots, citrines, garnets and aquamarines.

Made out of silver, brass, copper and steel.

Check out my Orchid Blog at
http://www.ganoksin.com/gnkurl/ep80je


#14

Fantastic Hans.


#15
Would someone let me know how to find this "fodiator" thing? What
day was it posted? I looked and can't find it. Sounds like it was
quite a hit!

Hi Marianne, I saved it so I can go back and look at it when I want
to smile, you’re going to love it.
http://www.ganoksin.com/gnkurl/ep80je

Thomas III


#16

http://www.ganoksin.com/gnkurl/ep80je

This is the link - make sure to scroll all the way to the bottom so
you don’t miss the video!


#17

$H*T, Hans, that’s awesome !.

sheltech.net


#18

Thank you for the info. Hans also sent the link to me. He is a
wonderfully mad, as you’ve all expressed so well!


#19

Hans… this is just incredible! You had to do this in anouther
life! Thanks for sharing! Chris