Back to Ganoksin | FAQ | Contact

That Dasterlly .. Porasity

Two major problems … at least for me … Casting (Going to
solve that by moving to Centrifucal Casting … as I should have
done years ago (so I’ve been advised! . . NOW!)


Number Two… Porasity… HOW DO U STOP IT!!

Really,… can we ‘ONLY’ hear from those who, "DO NOT HAVE IT
… CAUSE THEY KNOW HOW TO STOP FROM HAVING IT!! …

I have ideas as to the problem also… but I still have it so
guess my ideas are wrong…

How bout those speaking who don’t have the problem (less than
.5 percent of the time… answers from the masters… questions
from the humble masses) and questions from those who have the
progblem in spades(clubes, hearts, and diamond for me as
well!!)… questions.

GO NON-PEROSITY MASTERS . . SUDO-GODS AS U MAYBE!!) . . SPEAK TO
WE YOUR UNWASHED , UNEDUCATED, YET HUMBLE SERVANTS(SERIOUSLY)

Thanks,

Jim

Jim, I have a slightly used Neycraft spincaster I’m selling for
$325+shiping. you can contact me offline at
@jahenkel J.A.