hi there, what im looking for is way to find something that i can
put, like a paste on my glass cabs, to make a sort of textured
bezel,something that will work as a stong bail as
well,thanks,rodney
Hi Rodney -
This is an excellent application for PMC. I haven’t tried using the
paste version of it, but I have used the clay version of it to do
exactly this. You can fire it with the glass cab in place, and it can
be used as a bezel as well as a self-bail.
Linda
thank you for your response on the pmc,what i think i need is
something that would be cheaper,my things are for low end
buyers,maybe i just need to upgrade my line,thanks so much for
your reply,rodney