Hello again, experts. First of all I want to say thank you for all your previous advice on the casting problems I was having; your insights helped clear things up and I’ve had no problems since then.

My question has to do with the Tabletop casting oven, in particular the smallest one with a 6 x 6 interior floor space. I’ve been doing just one flask at a time, with a 5 hour run time, and have had no problems so far. What I’m curious about is if I cram another flask in there. The space inside is just large enough to fit two mall flasks, but is it SAFE to do so? Will the little ceramic stand hold all the wax runoff until it steams off? Is that tiny space ok for two flasks or should I just keep doing what I’ve been doing? Thanks in advance..

John at13th Floor

1 Like

I think it’s fine to cram another flask in there, as long as they don’t touch the elements.

Your question about whether the ceramic stand will hold all of the molten wax, depends on how much molten wax there is.

Does that help?

Yes it does. THANK YOU. Got a bunch of orders and need to punch them out, so this works. :grin: