Hi There,

I was wondering if any one may have advice on how to remove surface
tack from Colores Doming Resin. I poured the resin two days ago and
it is mostly cured but the surface appears a bit rubbery and tacky.
It is a bit humid here. I dont know if that makes a difference or
not.

Thanks in advance for any suggestions you may have.

Christine
www.christinebossler.com


#2
I poured the resin two days ago and it is mostly cured but the
surface appears a bit rubbery and tacky. It is a bit humid here. I
dont know if that makes a difference or not. 

I believe that means it will never cure up, and you need to dissolve
the epoxy out with Attack (OUTSIDE!) and re-do it.

I have found that putting a lamp down close to the epoxy helps get
the bubbles out.

You can also call Rio and ask for tech support, they answer
questions about their products.

Elaine