never ever ever stretch a ring with stones in it
if the shank is of a quality thickness say 2 mm aka built to last it
can be planished up 2 sizes and filed sanded and polished. Will
still have a 1.5 mm thick shank and work hardened.
all the best
Richard
Reality, most womens wedding rings eventually will need to be
re-sized due to pregnancy…
I must have been lucky then. Four children and my wedding rings still fitted the same afterwards. Now middle age spread - that's a different story! I've had to size up my wedding rings a couple of times in the last eight years.
Yeah, Shannon, I was stepping in it, having a retail store for 24
years, not much experience…
Helen, “Except not the rule”…
You take a piece of pvc pipe with an outside diameter a little bigger than the band. Cut a length a hair wider than the band. Trim the outside of the pvc section into a cone that fits into to shrink plate hole desired. Trim the inside of the pvc section into a cone that allows the band to fit mostly inside, a tight fit. It ends up fairly thin.