Dear Team,

Is it possible to use the White topaz stone for the wax setting
process? Then what’s the parameter need to fallow for the same.

Thanks & Regards,
Arulkumar Nallasamy

Dear Arul,
No it cannot be cast in situ
Umesh

Arulkumar

There are three colours of the American Flag, Red, White & Blue or
Ruby, Blue Sapphire & Diamond. sometimes CZ’s. anything else aren’t
gonna make it through the wax-setting process.

As for very soft White Topaz; don’t even think of it. Only as long
as its into the 9.0+ on the “Mohs’ Scale, of Hardness” will ‘Wax
setting’ work…