Can you steam the new resin waxes out of your flasks prior to your burnout? If so, is it recommended?
Unfortunately no. Wax will liquefy and trickle out of the mold when the steam heats it up, eliminating a lot of smoke if it doesn’t stay in the kiln. But resin just sits there in the mold.
1 Like