Steam Dewaxing


#1

I just used my $17.00 “Presto Kitchen Kettle” to steam dewax my
flasks in order to do a low temp casting. Works beautifully.


#2

Yep, and a &10.00 Crockpot makes a great pickle pot; put a glass
jar inside for the pickle, and fill the crockpot with a water and
baking soda solution to neutralize the pickle. I’ve been using
one for 6 jewelers for 5 years.