Hello everyone and I need some help restoring my stainless steel
shot. A friend of mine that owns a bead shop wanted me to clean some
chain for her that was getting tarnished. She said it was sterling.
I tossed it in my vibratory tumbler and when I took it out it was
pretty obvious it was not sterling and the finish on the chain was
coming off. I told her it was junk and she did say it was very
inexpensive and she bought it off of ebay from china. So, no good
deed goes unpunished: my shot is now turning everything a pretty
golden, brown. Not really what I am looking for. How do I get it out
of all of my shot?? I have roughly 25lbs of it? Any help is
appreciated. Thanks so much. :slight_smile: