hello orchid, I am looking for a new source of white topaz to use as
accent stones, sizes 1.5mm through 3mm. If anyone knows a good source
let me know my email is @eclipse_designs

thanks
sarah

Hi Sarah, I,ve real difficulty sourcing white Topaz, because
everyone wants to turn it blue, but you can take the blue and heat
it in a test tube over a alcohol lamp and just let it cool naturaly,
and it turns back to white, Paul

Bensel