Hi everyone:

This is my first post here in a few years! I am looking for a
supplier of stainless steel cable,multistrand stainless neckpieces as
well as rubber cords with stainless steel cables running inside the
rubber. I have seen similar items from Teno but I need a wholesale
supplier, if anyone knows of a supplier I would be VERY greatful!
Thanks in advance!

Cary James


#2

Cary

Downeast Trading Company, Middlebury VT 800 626-5700 has a nice
selection of multi-strand cables in stainless, black, and now in a
host of very hot colors. You should also contact Chris’s Cables,
Baton Rouge, LA 225 929-6964. They do multi-strand cables in a
variety of materials, including niobium. Since they make their own
cables, they are also able to do custom lengths. Both companies are
great to work with.

Doug

Douglas Zaruba
33 N. Market St.
Frederick, MD 21701
301 695-1107
@Douglas_Zaruba