Back to Ganoksin | FAQ | Contact

[Source] Sand casting equipment


#1

Greetings,

Anybody know of a company still selling sand casting equipment like
Allcraft did?

Bill in Vista


#2

I don’t know what Allcraft sold but here is a place to get almost
anything you could wand for a small sand casting foundry.
http://budgetcastingsupply.com/ All the prices listed include
shipping.

Brian


#3
Anybody know of a company still selling sand casting equipment
like Allcraft did? 

Try Kingsley North. They still sell the Procraft kit, so does
Monsterslayer.com

Ron Charlotte – Gainesville, FL
@Ron_Charlotte1 OR afn03234@afn.org


#4

Indian Jewelrs Supply out of Gallup N.M. sells the sand casting
equipment, sand and frames.

Sam Patania, Tucson
www.patanias.com