Hello everyone!! Im looking for a rubber necklace ( black ) 3 or 4 mm
in a 20’’ & 22’’ in length complete with 14k caps and lobster. Anyone
know where I can get this? Thanks

Cecena’s Jewelry
Antonio Cecena
http://www.CecenasJewelry.com


#2

HI, look in the Rio catalogue… Allcraft has nice ones with a great
clasp smooth… turn and lock… calgang and he also was supposed to
get them in colors… (rubber)


#3

Allcraft in New York, don’t have the address in front of me at this
moment. They have a selection of cord and clasps.