Back to Ganoksin | FAQ | Contact

[Source] Gold filled quality stamp

I have been making some gold filled pendants, and would like to
stamp them on the back with a 1/20 -14K GF stamp, but have been
unable to locate a source for the stamp. I checked with Rio and Otto
Frei, but neither carry them. If any of you can suggest a source I
will appreciate it. Alma

Alma-

Both Sossner Stamps and Alpha Tool, Die provide hallmark stamps.

They custom-make them as well.

Cheers.
Kim
KimEricLilot.com

Alma - You might try Harper Manufacturing
http://www.ganoksin.com/gnkurl/ep805v

You may have to get 2-3 stamps to create all of your hallmark.

all the best,
-Kim