Soldering with Propane torch in the house

I know this is late, but I have not paid any attention to this list
(and most every other) for a while. I am tiered of the same reply,
but understand what kind of a problem this is for some, please
contact the agents/dealer for more questions.

You can get a torch that will run off of a disposable propane can
that is not only suitable for casting, but is hot enough to alloy
gold or silver, and is good for both fine work and general
selversmithing (construction, including belt buckles). This is a
very nice product, in my opinion, I have no financial (or other)
interests in the product/company etc. I do not know how long a 1-lb.
can lasts, but it is a very long time. (Ain’t cheap, thanks to the
record low dollar.) See agents

http://www.planert-jewellery.com.au/precision_lp_gas_torch.htm

You will want all three tips, and need a 0-60 psi regulator. Due to
government regulations (US) the manufacturer will not ship directly.
(So much for “free trade” as China has no such barrier, i.e. the US
wants insurance as if this were a canister of gas, as in acetylene
etc., prohibitively expensive. Mine was shipped from Germany, but
“free trade” or is it Wally’s world policy kicked in. Can be shipped
from Australia, our government is not mad at them, yet.)

Student or other in need of something less than $100, that is
decent? See shark torch, Otto Frie is selling the EZ torch (same
thing) for $89.

This is not all that bad, although it is not in the liege as the
above, and has limitations. This is the low down on this (Did think
of getting one a long way back, found someone who used it in a class
they taught (insurance problem with acetylene.)

Do small butane soldering torches work?

Question, Edited:

I hope this is not a bother, but as you have no financial
interest in the matter, i.e. do not sell the item, I hope you may
give me an honest answer. I saw your Orchid post regarding the
Shark torch. I know you gave it a thumbs up, but I need to know,
and this is important, what limitations this torch may have. As
for myself, I cut rock. I also have got involved in
silversmithing, belong to a rock club etc. What I need to know is
if this torch can do large pendants, bracelets, and belt buckles
and bolos. The last two, if it struggles a bit but will do it may
be acceptable if it is not in the realm of ridiculous. 

Reply, Unedited:

Honesty, no problem! The Bernzomatic is a piece of crap,
wouldn't use it to burn down my house, let alone jewelry! The
Shark torch comes with three tips, from quite fine for small
stuff to large for much bigger jobs. I use a firebrick surround
when I'm doing big jobs, which helps bounce the heat back at the
object. Unfortunately, belt buckles and large bracelets are tough
with most torches, and honestly, I end up using two of them when
I do stuff that big. I can easily do bolos, and large pendants,
but I think the heavy weight of belt buckles might be
prohibitive. Now, if you have a Bernzomatic, you can use that in
one hand to keep the heat up in the whole piece and use the Shark
as the main focus for the actual soldering. It ends up being a
bit awkward, but it certainly works, and is definitely cheaper
than an acetylene set up. It is important to use the firebrick
surround, keeps the heat up, otherwise you're fighting a losing
battle. So in summary, it's not in the realm of ridiculous, by
any stretch, just needs an extra boost of heat to speed up the
process. In all other applications, I am quite happy with it,
especially due to the cost and the fine point flame available. 

Hope this may help someone, or satisfy curiosity.