Hello All,

What type of solder should one use with Shibuichi? I’m concerned
about the solder matching the color of the Shibuichi.

Mine is composed of one part silver and three parts copper.

Thanks,
Chris

Hi Chris,

A friend of mine had the same issue, the solder wasn’t the problem
(his solder technique is flawless), his problem was that the pattern
of the mokume didn’t match up.

His solution was to put “something nice” over the join.