Silver Sandcasting

Beginner in the delft clay sandcasting method of silver. Goal to learn wax carving for models and processes to create rings and pendants for necklaces.

Good luck! Delft Clay is a lot of fun to work with and fairly easy to learn. It is a bit expensive. If you are casting a piece where the finish isn’t important or an ingot, try using Petrobond. You can find it on Amazon. I have a very short PDF on my website where I Delft Clay cast a fossil impression. You can also search for Hans Meevis. He has a lot of really great tutorials. As I recall, one is how to use Delft Clay…Rob