I’m researching silver electroforming process. I would like to know
how I can get all equipments, such as anode, solution and bath for
silver electroforming at a really low price. I can’t afford to buy
electroformer at nearly $2000. Is there anyone who can tell me how
I can facilitate them?

Greetings: You can build your own rectifier at around $100. Chemicals
are easily available from various sources. The only reason though I
replied is that unless you are fully conversant with silver
electroforming take great care because generally silver
electroplating and forming chemicals are CYANIDE based and can KILL
you if you do not know exactly what needs to be done.

Regards,
Joe Bokor
jkbokor@telus.net