In February of this year I purchased 7 floor cases and 2 wall cases
from Citishowcase and Display. I am not a high traffic store so the
problems I am having seem to be of great concern. The cases are
veneer and the veneer seemed very thin when they arrived. I now have
2 cases where the veneer is buckled and cannot be flatted down. Does
anyone have a suggestion. I have had many other problems with these
cases this is just the latest one. If ever the adage about getting
what you pay for applies, I have truly learned my lesson.

Michael Parsons
Michael’s Jewelry