Setting stones with large pavilions

When setting stones with large pavilions, test fit the stone table
down. When the stone fits in the seat table down, you can be certain
the seat is cut properly to accommodate the girdle of the stone.
Then all remaining cutting on the prongs needs to be done below the
girdle to accommodate the pavilion

Brad Simon CMBJ