I wonder if a member would be willing to share how they set princess
cut stones all next to each other with no metal in between? I have
seen this done in a heart, for example, where the stones look like
they are butted right up against each other. How do they stay in?

Thanks again for your willingness to share your knowledge.

Mary Barker


#2

Hi Mary, The possible techniques are called bead, flush, pav=E9 or
invisible setting.