[$Sale] neglected rolling mill


#1

i have in my possesion a rolling mill that got ignored for long enough to
allow corrosion to settle lightly on the actual “rolls”. i’ve used a
dremel with a stainless brush to clean off most of it, but i fear there
might be irregularities now. is there a way to get it refinished? does
anyone want to buy it as is? it’s got both flat and square wire pressing
surfaces and is about 20 years old. it’s still gonna be here for the next
1000 years…i’m sure someone can use it!
thanks Holly


#2

Hi Holly,

To refinish rollers on mill: Take the rollers to a machine shop. Explain
that you need them to be ground down the same amount on each roller, then
case hardened to .045".

Best Regards,
Elaine Corwin
GESSWEIN CO INC USA
Tech Support : 1-800-544-2043 ext. 287
Tel: 203-366-5400

Elaine Corwin