g’day Lin I use a variety of resin sytems including the ubiquitous
Ceramit, 3M’s Filtek (UV curing dental composites), ordinaryish
two-pack casting epoxies, and UV and thermosetting acrylics.

What I use depends on the particular job in hand. Were these pieces
of which you speak made by your friend or are they work she has taken
in for repair?

What I do as well is explain to my clients before I perform any
repair work with resins exactly what it is they are getting for their
money and what they can reasonably expect in the way of material
performance.

Cheers
Al Heywood