Oooh yes I see! Logical! Well I will make new ones then. Thank you very much Rob! Your advice is highly appreciated!
I would likely do that too…Rob
1 Like
Since you already have the bezels made, you might try again with 1, using medium solder, but paying very close attention to your bezel seam, and avoiding lingering with the torch or using any excess heat in this area. You now recognize the risks, and what to watch out for.
Just a thought.
2 Likes
Thank you too ringdoctor!