I had an idea. That sentence usually strikes terror into the hearts
of normal persons. My waxes get tiny little fuzzy dust stuff wedged
into the smallest places in my pieces. Hours with a dental pick bored
me silly. So, what was the solution? Put it in ultrasonic cleaner, no
heat, water only and in less than a minute the crevices are clean!!!
Egad but I DO love toys.