Hello everybody,

First I want to say Happy Thanksgiving to you, then my question; My
daughter brought me silver precious metal clay 3-4 years ago. I
didn’t do anything with it. I wanted to use it the other day and I
found out that it became very hard. Does anybody have any suggestion.
I have never used and don’t know anything about PMC.

Thank you very much in advance.
Kind regards,
Oya Borahan

I wanted to use it the other day and I found out that it became
very hard. Does anybody have any suggestion. I have never used and
don't know anything about PMC. 

Great timing, I just posted the answer to this on my blog today.

Yes, you can turn it back into clay. But I wouldn’t want to start
with PMC using reconstituted stuff. I would suggest you buy fresh,
get a feel for how it should feel, then reconstitute and use the old
stuff.

Elaine
http://www.CreativeTextureTools.com