Hai,

We are producing 14kt yellow & white gold products. While doing
soldering the 14kt solder is not flow-able and it very ductile.

We were faced the following problems.

  1. We made trial it is not ductile but whereas the flow-ability is
    poor.

  2. In the second trial it is very ductile and the flow-ability is
    good.

Give your valuable suggestion…

Thanks & Regards,

kac
Ped-Jew