Thank you Joe.

I appreciate your advise.

You’re right, we don’t have the fume venting equipment yet. We
should. We will.

I have proven that the metal is good, but, after pouring into water,
the color of the shot was very dull, grey like lead. I suppose is
like firescale, and it should get better with the pickling and the
tumbling. Am I right? What else do you think I should use?

Thanks again.