Is electopolishing (stripping) the article an option? It will
bring a high polish to the item, but removes metal randomly. I
would suggest contacing your friendly electroplater for advice,
as there are many dangerous/ hazardous cemicals and acids
associated with this process. There are many books on
electroplating that would explain this process in more detail if
you need to find out more about it yourself. Hope this helps,
Linda