Dear Sir,
I would like to know from your great experience that how do I
recover Gold from Silver Chloride. I had refined Gold by Aqua
Regia and than there was Silver chloride which had come out from
the Process. Now i have app.775 gms of Silver Sludge and according
to my Lab there is 76% Gold in it. So please let me know How do
I recover Gold from this Chlorides.I would appreciate if you
could send us some details in this context. Your information
will be of great help to us.

Regards,
Pulkesh Patel.